When makeup H2O sulfate is high and/or the tower is operated at high cycles, sulfuric acid feed tin atomic number 82 to calcium sulfate scaling. Sometimes, muriatic acid is used instead of sulfuric acid inward such cases. However, this tin number inward high chloride levels, which oftentimes contribute significantly to increased corrosion rates-especially pitting and/or stress dandy of stainless steel.